Various commercially available zeolite frameworks (MFI, FER, BEA, MOR, FAU) with iron impurities ranging from 85 to 780 ppm and nominal Si/Al ratios of 10-15 have been tested in direct N2O decomposition after calcination and steam treatment. Our results show a significant impact of the framework type on the catalytic activity at these high degrees of iron dilution (Fe/Al < 0.01). H-beta was the most effective material in the reaction, followed by the other pentasyl-type H-ferrierite and H-ZSM-5 zeolites.
A. H. Øygarden, J. Pérez-Ramírez
Appl. Catal. B-Environ. 2006, 65, 163-167