We use cookies to help you navigate efficiently and perform certain functions. You will find detailed information about all cookies under each consent category below.
The cookies that are categorized as "Necessary" are stored on your browser as they are essential for enabling the basic functionalities of the site. ...
Necessary cookies are required to enable the basic features of this site, such as providing secure log-in or adjusting your consent preferences. These cookies do not store any personally identifiable data.
Functional cookies help perform certain functionalities like sharing the content of the website on social media platforms, collecting feedback, and other third-party features.
Analytical cookies are used to understand how visitors interact with the website. These cookies help provide information on metrics such as the number of visitors, bounce rate, traffic source, etc.
Performance cookies are used to understand and analyze the key performance indexes of the website which helps in delivering a better user experience for the visitors.
Advertisement cookies are used to provide visitors with customized advertisements based on the pages you visited previously and to analyze the effectiveness of the ad campaigns.
Other cookies are those that are being identified and have not been classified into any category as yet.
Metal oxides and oxyhydroxides exhibit state-of-the-art activity for the oxygen evolution reaction (OER); however, their reaction mechanism, particularly the relationship between charging of the oxide and OER kinetics, remains elusive. Here, we investigate a series of Mn-, Co-, Fe-, and Zn-doped nickel oxides using operando UV–vis spectroscopy coupled with time-resolved stepped potential spectroelectrochemistry. The Ni2+/Ni3+ redox peak potential is found to shift anodically from Mn- < Co- < Fe- < Zn-doped samples, suggesting a decrease in oxygen binding energetics from Mn- to Zn-doped samples. At OER-relevant potentials, using optical absorption spectroscopy, we quantitatively detect the subsequent oxidation of these redox centers. The OER kinetics was found to have a second-order dependence on the density of these oxidized species, suggesting a chemical rate-determining step involving coupling of two oxo species. The intrinsic turnover frequency per oxidized species exhibits a volcano trend with the binding energy of oxygen on the Ni site, having a maximum activity of ∼0.05 s–1 at 300 mV overpotential for the Fe-doped sample. Consequently, we propose that for Ni centers that bind oxygen too strongly (Mn- and Co-doped oxides), OER kinetics is limited by O–O coupling and oxygen desorption, while for Ni centers that bind oxygen too weakly (Zn-doped oxides), OER kinetics is limited by the formation of oxo groups. This study not only experimentally demonstrates the relation between electroadsorption free energy and intrinsic kinetics for OER on this class of materials but also highlights the critical role of oxidized species in facilitating OER kinetics.
Rao, R. R.; Corby, S.; Bucci, A.; García-Tecedor, M.; Mesa, C. A.; Rossmeisl, J.; Giménez, S.; Lloret-Fillol, J.; Stephens, I. e. L.; Durrant, J. R.
J. Am. Chem. Soc. 2022, 144 (17), 7622–7633
DOI:
10.1021/jacs.1c08152